Pomalux ® is a high-performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even machining parts with complex geometries. Pomalux ® is an excellent choice for many bearing and wear applications since it has low coefficient of friction and wears well in both wet and dry environments. It is widely used for assembly jigs and fixtures because of its inherent dimensional stability and excellent wear properties.
Pomalux ® is often specified for electrical applications when low moisture absorption and high dielectric strength are required. Both natural and black Pomalux ® are FDA compliant for use in food processing machinery.
• High strength and stiffness
• Low friction
• Easy to machine
• Good dimensional stability
• Low moisture absorption
• Resists abrasive wear in both wet and dry environments
• Good chemical resistance
• Excellent electrical properties
• FDA compliant
Contact us today for your fabrication and machining needs!
Request Fabrication/Machining ServicesFeatured Download
Available In
Sheet, Rod, Tube, Film
Certifications
FDA Compliant, ITAR Registered
Start Your Quote
Send us a message:
*Required Fields
Type | Size | Length | Color |
---|---|---|---|
Sheet | .060 – 6” | 24” x 48’, 12” x 48”, 48” x 96” | Natural & Black |
Rod | 1/8” – 12” | 96”, 120” | Natural & Black |
Tube | ½” – 4” ID | 120” | Natural |
Film | .010 – .060 | Natural & Black |
Give us your cut-to-size dimensions. We will precision-cut these plastics to your exact size. Additional sizes and colors available upon request.
Physical Properties | Units | ASTM | Results |
---|---|---|---|
Density | lb/in³ | D792 | 1.41 |
Water Absorption, 24 hrs | % | D570 | 0.22 |
Mechanical Properties | Units | ASTM | Results |
---|---|---|---|
Tensile Strength @ yield | psi | D638 | 8,800 |
Tensile Modulus | psi | D638 | 410000 |
Tensile Elongation @Break | % | D638 | 30 |
Flexural Strength | psi | D790 | 12 |
Flexural Modulus | psi | D790 | 375000 |
Compressive Strength | psi | D695 | 16000 |
Compressive Modulus | psi | D695 | 400 |
Hardness, Rockwell R | D785 | M80 | |
IZOD Impact Strength Notched | ft-lb/in | D256 | 1.2 |
Thermal Properties | Units | ASTM | Results |
---|---|---|---|
Coeffcient of Linear Thermal Expansion | (x 10^-5 in./in./°F) | 4.7 | |
Heat Deflection Temp at 264 psi | °F | 219 | |
Thermal Conductivity | BTU-in/ft²-hr-°F | 1.6 | |
Thermal Conductivity | BTU-in/ft²-hr-°F | 1.6 | |
Flammability Rating | HB |