Hydlar™ ZT has the added benefit of a small amount of PTFE added for increased lubricity (lower friction) resulting in improved wear resistance. This material makes it possible to achieve low abrasiveness without sacrificing low wear rates. Hydlar™ ZT’s tough, strong reinforcing material makes the end product extremely wear resistant without excessive galling to mating wear surface.
Contact us today for your fabrication and machining needs!
Request Fabrication/Machining ServicesGeneric Name
Aramid Reinforced Polyamide
Available In
Sheet, Rod
Start Your Quote
Send us a message:
*Required Fields
| Type | Size | Length | Color |
|---|---|---|---|
| Sheet | .25″ to 2″ | 24” x 24” CTS | Tan |
| Rod | .25″ to 5″ | Varies by diameter | Tan |
Give us your cut-to-size dimensions. We will precision-cut these plastics to your exact size. Additional sizes and colors available upon request.
| Physical Properties | Units | ASTM | Results |
|---|---|---|---|
| Density | lb/in³ | 1.16 |
| Mechanical Properties | Units | ASTM | Results |
|---|---|---|---|
| Tensile Strength @ yield | psi | D638 | 16000 |
| Tensile Modulus | psi | D638 | 130000 |
| Tensile Elongation @Break | % | D638 | 4 |
| Flexural Strength | psi | D790 | 23000 |
| Flexural Modulus | psi | D695 | 900000 |
| Compressive Strength | psi | D695 | 19300 |
| IZOD Impact Strength Notched | ft-lb/in | D256 | 2.7 |
| Thermal Properties | Units | ASTM | Results |
|---|---|---|---|
| Coeffcient of Linear Thermal Expansion | (x 10^-5 in./in./°F) | 1.6 | |
| Heat Deflection Temp at 264 psi | °F | 470 |
| Electrical Properties | Units | ASTM | Results |
|---|---|---|---|
| Dielectric Constant @1 MHz | 2.5 | ||
| Dissipation Factor@1 MHz | 0.0016 | ||
| Volume Resistivity, 50% RH | ohm-cm | 2000 |